A compression-moulded part depends on, well, compression.
For thermoset components, pressure forces the material into shape while heat initiates and accelerates curing. So, why would a manufacturer briefly reopen the mould, sometimes several times, before that cure is complete?
This controlled movement is known as ‘breathing’. It may last only seconds, yet it can influence whether your component meets its surface finish, dimensional tolerances and performance requirements. The difference between an effective breathing step and a damaging interruption depends on what’s happening inside the cavity and exactly when the mould opens. To understand why, we first need to look at what can become trapped inside a closed mould.
How does trapped gas affect compression-moulded parts?
Unless the process uses vacuum, air is present in the open mould before the charge enters. It can also become trapped between pieces of material, between particles in granular compounds or among the fibres and layers of a composite charge.
Some thermosets also release volatile substances as they warm and cure. Residual moisture may turn into vapour. The combination depends on the compression moulding material, its formulation, storage and preparation.
As the mould closes, the flowing charge displaces the air and gases and directs it towards the tool vents. However, the material may surround a pocket before it can escape. This is harder to control when the component has deep features, inserts and converging flow fronts.
Gas left inside the component may form a void or low-density area. Near the surface, it can create a blister. Highly compressed and heated gas can also leave a porous, dull or scorched mark. If a pocket prevents material from reaching part of the cavity, you may see a non-fill or poorly formed feature.
How does breathing release trapped gas from the mould?
During breathing, the press briefly releases pressure or opens the mould by a controlled amount. The compressed gas can then escape towards the lower-pressure area outside before the mould closes again.
The mould may ‘breathe’ once or several times during each compression cycle, depending on the component, material and tooling.
Importantly, breathing isn’t the same as conventional mould venting. Vents are permanent shallow passages built into the tool, often at the parting line or around an ejector pin. Breathing is a timed press movement that briefly releases pressure or separates the mould halves. In simple terms, vents provide fixed escape routes, while breathing creates temporary pressure relief that helps drive air and volatiles towards those routes. Our introductory guide explains what breathing is in compression moulding.
When should breathing happen during the moulding cycle?
Creating that escape route isn’t enough. The mould must also reclose before curing has progressed far enough to restrict the compound’s flow.
A breathing step only works while the compound is still able to flow and consolidate when full pressure returns. Once the press recloses and restores the required moulding pressure, the normal compression cycle continues as the material forms and cures inside the cavity.
If the mould stays open for too long or curing advances too far before full pressure returns, separate areas of material may not knit together properly when pressure is reapplied. As a result, poorly timed breathing can create weak areas rather than improve quality.
Which factors determine the breathing cycle?
The timing, opening distance, duration and number of breathing cycles depend on the resin chemistry, charge preparation, component thickness, mould temperature and press. Manufacturers establish the settings through material guidance, mould trials, inspection and production experience.
Tool design also influences where gas collects and how it escapes. Addressing vent locations, parting lines, inserts and difficult cavity features during design and tooling reduces the need to correct avoidable problems after production begins.
Why can’t breathing prevent every moulding defect?
A breathing cycle isn’t a cure for every void, blister or non-fill. The manufacturer must also control charge weight and position, material condition, closing speed, temperature, pressure and cure time.
The vents must lead to the atmosphere and technicians must keep them clean and clear. If they’re blocked, gas may remain trapped inside the mould. On the other hand, vents that are too deep may fail to seal as material enters them, leaving insufficient cavity pressure to correctly form the part.
Control quality throughout the compression moulding process
By releasing trapped air and volatiles at the right point in the cycle, breathing can reduce gas-related defects and support consistent dimensions and performance.
But breathing works only when it suits the material, geometry and tool. At Talisman Group, we help you consider those factors from component development and tooling through to mould trials and repeat production. Our manufacturing facility operates an ISO 9001:2015-certified quality management system, supporting controlled processes and consistent production.
Contact us to discuss your drawings, material requirements and quality criteria with our compression moulding team.